Owing to the high levels of mechanical properties (in particular, high-temperature, strength) and electrophysical properties, densely sintered mullite ceramics are finding ever increasing engineering applications. Sol-gel technology is one of the promising methods for obtaining mullite ceramics with a wide range of compositions and properties at low sintering temperatures.
Origin
Unknown
Journal Title
Glass & Ceramics 46 8 1989 340-342
Sector
Glass Ceramics
Class
GC 150