The crystallisation heat treatment process was investigated and optimised for an antimony containing slag glass ceramic. The appropriate heat treatment conditions were determined using the orthogonal design method and with the aid of differential thermal analysis.
Origin
Human University, China
Journal Title
Glass Technology 36 2 1995 61-64
Sector
Glass Ceramics
Class
GC 187