The corrosion of 6 different refractory candidate materials was studied using a modified ASTM C621 method for a DC-plasma arc furnace processing mixed waste.
Origin
Pacific Northwest National Labs, Usa
Journal Title
Ceramic Trans 82 1998 385-400
Sector
Refractories
Class
R 315