The crystallisation of cordierite glass and cordierite-based oxyfluoride glasses was studied by differential thermal analysis and X-ray diffractometry.
Origin
Rensselaer Polytechnic Institute
Journal Title
Phys Chem Glasses 1989 30 3 95-102
Sector
Glass Ceramics
Class
GC 46