Cordierite-based oxyfluoride glasses were prepared and various of their properties measured. The glasses were used to produce glass ceramics which may have practical applications as packaging materials for electronic devices.
Origin
Rensselaer Polytechnic Institute
Journal Title
Phys Chem Glasses 1989 30 3 86-95
Sector
Special Glass
Class
S 262