Glass is one of the most difficult properties of a leadless glaze to adjust to a product specification. A high gloss is difficult to achieve because of the relationship between specular gloss and atomic number. A matte glaze requires reproducible control of a crystallisation process during firing.
Origin
Appler Associates, Cheshire, Ct, Usa
Journal Title
Ceram Eng Sci Proc 16 1 1995 40-45
Sector
Glass Ceramics
Class
GC 214