The basicity concept, elaborated by the author, is presented together with the natural basicity scale of pB. The possibility of correlating and predicting glass properties by means of pB is emphasized. The application to chemical interaction confirms a new way for matching a refractory material to a given glass melt or a glass composition to a given reaction medium, in order to diminish the interaction intensity.
Origin
Uuniv Politechnica, Bucharest, Romania
Journal Title
Proc Xvii Icg, Beijing, 3 Glass Properties 1995 27-32
Sector
Special Glass
Class
S 1274