A new full-thickness gunnable foam/fibre insulation system provides a fast, effective alternative to traditional modules and blankets of furnace-lining maintenance.
Origin
Unifrax Corp, Usa
Journal Title
Am Ceram Soc Bull 81 11 2002 31-33
Sector
Refractories
Class
R 452