A generalised criterion for evaluating the quality of glass property calculations is proposed. This criterion permits the comparison of the quality of existing methods of calculation of a given property in a given composition area. Values for ten of the most well known calculation methods and a new method by Priven are compared. The SciGlass Information System containing experimental property data for more than 130,000 glasses was used. Recommendations concerning the selection of the best methods of glass property calculations in various composition areas are made.
Origin
Thermex Co, Russia
Journal Title
Glass Technnology 44 4 2003 156-166
Sector
Special Glass
Class
S 2718a