The effect of phase separation on viscosity of glasses is discussed with reference to a recent article by Simmons and Simmons (Am Ceram Soc Bull 1989 68 11 1949).
Origin
Ibm Research Division, Rensselaer Polytechnic Institute
Journal Title
Ceramic Bulletin 1990 69 9 1506-1507
Sector
General
Class
G 480