Cathodluminescence microscopy is an inexpensive characterization technique to determine phase identification, distribution and quantification of refractory raw materials and products.
Origin
University Of Missouri-Rolla, Usa
Journal Title
Am Ceram Soc Bull 77 6 1998 55-61
Sector
Refractories
Class
R 281