It has been shown that reboil on reheating to the temperatures required for lamp working can be prevented by subjecting the nitrided porous glass to chlorine at elevated temperatures prior to pore closure.
Origin
Corning Glass Works
Journal Title
Glastech Ber 1988 1 24-28
Sector
Special Glass
Class
S 145