Experiences in the application of chimney block packing in glass tank regenerators are reviewed with reference to their advantages over straight conventional packings.
Origin
San Miguel Packing Products
Journal Title
Glass International March 1991 41, 43, 45, 47
Sector
General
Class
G 568