Chemical Treatment Of Glass Substrates

The effects of cleaning on the near-surface composition of Corning Code 1737 glass was studied.

Author
J Gregory Couillard Et Al
Origin
Cornell University, Usa
Journal Title
Corning Research 1997 7-12
Sector
Special Glass
Class
S 1422