To obtain separate measurements of charge carrier concentration and mibility, isothermal curve limiting slopes have been studied on the (xLi2O, (1-x)Ag2O)-P2O5 glassy system which shows a strong mixed alkali effect.
Origin
Inpg/Cnrs
Journal Title
Phys Chem Glasses 1990 31 3 98-102
Sector
Special Glass
Class
S 400