Ceramics serve a crucial role in enabling developments in the electronics industry through their essential role in the manufacturing, use, and application of advanced semiconductors.
Origin
Kyocera International
Journal Title
Am Ceram Soc Bull 97 3 2019 32-39
Sector
Glass Ceramics
Class
GC 917