High-temperature ceramic coatings for furnace-lining refractories can simultaneously reduce energy consumption, improve temperature uniformity, reduce furnace maintenance, and increase production, as this paper explains.
Origin
Int Tech Ceramics Llc, Usa
Journal Title
Am Ceram Soc Bull 97 3 2019 48-51
Sector
Refractories
Class
R 931