[Case Report] Injuring Potential Of Drinking Glasses

At a party of a sports club, an argument started between two groups of young men, in the course of which one of the persons involved threw a beer glass hitting a young man of the other group, who collapsed with a profusely bleeding wound. Although resuscitation measures were initiated immediately, the victim died at the scene due to exsanguination from the completely severed left external carotid artery in combination with the aspiration of blood. Tests with drinking glasses thrown at a skull-neck model suggested that an undamaged beer glass thrown at the head of the victim could not cause the fatal injuries on the neck because of its splintering behaviour. In fact, it seemed that the beer glass had been damaged prior to throwing and that its sharp edges perforated teh skin on hitting the neck.

Author
V Sterzik Et Al
Origin
Inst Legal Medicine, Albert Ludwig University, Freiburg, Germany
Journal Title
Forensic Science International 179 2008 E19-E23
Sector
Domestic glass
Class
D 1284

Request article (free for British Glass members)

[Case Report] Injuring Potential Of Drinking Glasses
Forensic Science International 179 2008 E19-E23
D 1284
Are you a member?
This question is for testing whether or not you are a human visitor and to prevent automated spam submissions.
16 + 2 =
Solve this simple math problem and enter the result. E.g. for 1+3, enter 4.