The nonisothermal crystallisation of La(1-x)PrxBGe05 glasses with 0.00
Origin
P.Le Tecchio, Italy
Journal Title
Phys Chem Glasses 39 3 1998 151-153
Sector
Special Glass
Class
S 1437