The reasons why fast Fourier transform techniques have not replaced classical methods are discussed and conditions for using time domain spectroscopy for fast measurements on glasses are deduced.
Origin
Ura - Lab Sci Mat Vitreux, Montpellier
Journal Title
Riv Staz Sper Vetro 1990 20 6 185-190
Sector
General
Class
G 554