Boron Nitride - A Review

The chemical combination of boron and nitrogen does not occur in nature. This article discusses the properties, manufacture and applications for one of the key advanced ceramics in modern technology.

Author
D A Lelonis
Origin
Advanced Ceramics Corp
Journal Title
Ceramic Technology International 1994 57-58, 60-61
Sector
Glass Ceramics
Class
GC 140