To combine the mechanical properties of high-strength base metals with the biological properties of bioactive materials, coatings of BIOVERIT glasses and glass-ceramics on CoCr alloys and titanium have been produced.
Origin
Friedrich-Schiller Universitat, Jena, Germany
Journal Title
Glastech Ber Glass Sci Technol 68 4 1995 117-122
Sector
Glass Ceramics
Class
GC 184