The topography and nanostructure of several technical borofloat and soda-lime-silicate float glasses were investigated by a high-resolution atomic force microscope (AFM). The irregular ripple pattern to be seen on as-received atmosphere and tin bath side surfaces had an average diameter of ~60nm, heights
Origin
Inst Fur Nichtmetallische Werkstoffe, Germany
Journal Title
Glas Sci Technol 75 4 2002 174-183
Sector
Special Glass
Class
S 2386