There arc plasma spraying process is described, and examples of ceramic materials applications are presented. Some effects of powder materials characteristics on the properties of sprayed deposits are described.
Origin
Massachusetts Inst Of Technology & Avalon Materials Technology, Usa
Journal Title
Am Ceram Soc Bull 73 2 1994 45-50
Sector
Glass Ceramics
Class
GC 163