The use of EPMA in investigating glass defects is illustrated by reference to analysis of a zirconia stone. The analysis of a cordierite composite by this technique is also described.
Origin
Schott Glaswerke
Journal Title
Glastech Ber 1990 63 11 342-346
Sector
General
Class
G 513