The principles and measuring methods of FT-IR radiation spectrum are presented in this paper.
Origin
Qiqihar Inst Light Industry, China
Journal Title
Proc 17Th Int Cong Glass, Beijing, Vol 3,October 1995 233-238
Sector
Special Glass
Class
S 1284