Annealing stages are tabulated. The furnace is shown diagrammatically and the time temperature profile of the cycle is shown graphically over a period of some 26 months. Methods employed to achieve the required conditions are described.
Origin
Unknown
Journal Title
Soviet J.Opt.Technol., 43 12 1976 723-6
Sector
Primary Papers
Class
PP 1454