Electrical conductivity due to halide ions has been measured for the glasses in the system 30 SiO2.(70 - x)PbO.xPbX2 (0
Origin
Okayama University
Journal Title
J Am Ceram Soc 1988 71 10 864-868
Sector
Special Glass
Class
S 186