Three types of glass fibres, differing mainly in their alumina, alkaline earth and alkali oxide contents, were investigated by secondary neutral mass spectrometry.
Origin
Technische Universitat Clausthal, Germany
Journal Title
Glastech Ber Glass Sci Technol 72 7 1999 227-232
Sector
Glass Fibre
Class
GF 225