A stability analysis of the stationary drawing of optical fibres under isothermal and nonisothermal conditions was carried out in terms of the linear theory of hydrodynamic stability on the basis of a one-dimensional model.
Origin
Leningrad Institute Of Precision Mechanics & Optics
Journal Title
Glass Technology 1990 31 6 240-244
Sector
Glass Fibre
Class
GF 62