Modern instruments attain higher sensitivity and reproducibility. Details are given of the use of the Siemens and Halske multichannel kristalloflex IV for the complete analysis of dolomitic limestone or fledspar in 4 to 5 min. The closeness of the specimen to the window permits exposures as short as 1 min. The sample is ground finer than 16u in a hammer mill (1min). The calibration material must be carefully matched with the specimen.