The wettability of binary and ternary glasses belonging to Si02-Al203-Zr02 diagram has been studied using the sessile drop technique at 1750 & 1800 deg C.
Origin
Incar, Spain
Journal Title
Jacs 88 4 2005 1000-1003
Sector
Special Glass
Class
S 2936