A mechanized continuous line for the production of long-length hollow tube electroceramic parts is described. The line consists of an aoutomated complex for shaping and drying tubes, a glazing block, a roasting module, and a cutting lathe. The line makes it possible to automate the laborious operations of shaping, drying, glazing, and roasting.