1H Mas Nmr And Ir Studies On Powdred Alkali-Lime-Silica Glasses

Powdered samples of glasses with the composition 16 R20.10 Ca0. 74 Si02 (R=Na, K, Cs) and a concentration of water in glass of about 0.03 mol.1-1 were studied by solid state 1H MAS NMR (magic angle spinning nuclear magnetic resonance).

Author
W Storek Et Al
Origin
Bam, Germany
Journal Title
Glastech Ber Glass Sci Technol 73 12 2000 373-379