An X-Ray Photoelectron Spectroscopy Study Of Anion Bonding In Tin(Ii) Fluorophosphate Glass

An X-ray photoelectron spectroscopy is used to examine the structural environments of F and O in several series of SnF-SnO-P2O5 glasses.