X-Ray Diffraction Made Easy: New Xrd System

Various analytical methods can be used to characterise glass and ceramic materials, among which X-ray diffraction plays an important role. In addition to providing the overall structural information and its verification, XRD can be used to determine the crystallite size directly. This article presents some of the qualitative and quantitative XRD data on CuC204 in this context.

Author
J Muller Et Al
Origin
Thermo Arl, Switzerland
Journal Title
Int Ceramics 1/2003 36-39