Waterford Crystal Invests In Datapaq Technology For Process Monitoring

Waterford Crystal, based in the Republic of Ireland, has three manufacturing plants in the Waterford area. In recent recessionary times the company, like many other leading manufacturers, has invested in technology to trim losses and increase profits.

Author
D Plester
Origin
Datapaq
Journal Title
Glass Machinery Plants & Accessories Vii 2 1994 88-89