Voltammetric And Chronopotentiometric Reactions Of Silver Ions In Molten Sodium Disilicate Glass

Electrochemical reactions of silver species in molten sodium disilicate glass have been investigated by means of cyclic voltammetry and chronopotentiometry wothin the temperature range 900-1081 degrees C.

Author
M Maric, M P Brungs, M Skullas-Kazacos
Origin
University Of New South Wales
Journal Title
Phys Chem Glasses 1089 30 1 12-18
Sector
Special Glass
Class
S 215