Vaporisation Of Rubidium And Strontium From Borosilicate Glasses

A comparison is made between the vaporisation of rubidium and strontium from borosilicate glasses by a mass spectrometric Knudsen effusion method.

Author
M Asano Et Al
Origin
Kyoto University, Japan
Journal Title
Phys Chem Glasses 1991 32 6 258 - 262
Sector
Special Glass
Class
S 604