Use Of A Simplex-Lattice Experimental Design For Studying Glasses

A topical problem in glass technology is the development of compounds with specified properties for specific industrial purposes. As a rule, in such cases, the effect of each component on the physicochemical properties of the system is studied. The physical and chemical properties of a PKW (phosphogypsum-kaolin-waste) glass, using waste from a copper concentrating factory to obtain vitreous and glass crystalline materials with industrial waste as a basic ingredient, was investigated.

Author
M M Azizkhodzhaeva Et Al
Origin
Uzbek Republic Academy Of Sciences
Journal Title
Glass And Ceramics 49 7-8 1992 386-388
Sector
Special Glass
Class
S 902

Request article (free for British Glass members)

Use Of A Simplex-Lattice Experimental Design For Studying Glasses
Glass And Ceramics 49 7-8 1992 386-388
S 902
Are you a member?
This question is for testing whether or not you are a human visitor and to prevent automated spam submissions.
11 + 8 =
Solve this simple math problem and enter the result. E.g. for 1+3, enter 4.