Use Of Modern Domestically Produced Equipment In Glassmaking Practice

Positive experience in using modern Russian equipment - series LMO magnetic separators for quartz sand and a specialised magnetic holder for glass-molds for the production of glass containers - at the Smerdomskii Steklozavod is described. It is shown that the use of magnetic enrichment of quartz sand from a local deposit has a positive effect on the technological processes of glassmaking, and the use of specialised magnetic holder for glass-molds increases the repair quality and decreases repair time for glass mould.

Author
S E Karpushev Et Al
Origin
Smerdomskii Steklozavod, Russia
Journal Title
Glass & Ceramics 5-6 Sept/2011 156-158
Sector
Container glass
Class
C 4568

Request article (free for British Glass members)

Use Of Modern Domestically Produced Equipment In Glassmaking Practice
Glass & Ceramics 5-6 Sept/2011 156-158
C 4568
Are you a member?
This question is for testing whether or not you are a human visitor and to prevent automated spam submissions.
6 + 3 =
Solve this simple math problem and enter the result. E.g. for 1+3, enter 4.