The Use Of Lime-Silica Slag From The Phosphor Industry And Of Basic Slag For The Production Of Green And Amber Container Glass (Italian)

The effect of increasing amounts of slag on the melting rate is discussed on the basis of laboratory melts, which have also provided useful insight into the redox mechanism in the melting of green container glass.