According to the Chairman of Fuyao N America, which acquired a former General Motors plant in 2014, there will be around 1000 people working at the site by the end of 2015, which is 200 more than the previously expressed figure. In May 2014, auto glass producer Fuyao bought 1.2M sq/m of a former General Motors plant in Moraine, and the work of retrofitting the plant and preparing it for production is ongoing. The plant is expected to be completed by March 2015.