Us$15M Glass Factory Opens In Dubai

Alumcon, an aluminium facade contractor and glass manufacturer, has begun operations at its new $15M glass processing factory in Dubai. The new facility has a daily production capacity of 2000 square metres of insulated glass and 1000 square meters of frameless glass.