Ultrasound For Inspecting Glass Furnace Refractories

Glass refractory products with a high unit price are best investigated with non-destructive testing methods, ultrasonic forms of which can be used to determine material data and carry out quality control.

Author
B Fleischmann
Origin
Research Assoc Of The German Glass Industry
Journal Title
Glass Prod Tech Int 1996 60-62
Sector
Refractories
Class
R 193