Ultra-Clear Pv Glass Plant Boosts Chinese Production

A new production line at the Kibing Dongshan Glass Industrial Park in China was put into operation in September 2011, with a daily output of around 800/tpd of ultra-clear photovoltaic glass. With the total investment amounting to CNY 14BN, the industry park is thought to be the largest private industrial project in Jujian, China, built by the Ningbo Flat Foreshore Group. Since construction of the industry park in 2007, a high-quality float glass production line with a daily captaincy of 900/t, an online low-E coated glass line with a daily capacity of 600/tons, an online transparent conducting oxide (TCO) coated glass line with a daily capacity of 600/t and other supporting projects have also been put into operation.

Author
Un-named
Origin
Unknown
Journal Title
Glass Int Oct/2011 7
Sector
Flat glass
Class
F 3184

Request article (free for British Glass members)

Ultra-Clear Pv Glass Plant Boosts Chinese Production
Glass Int Oct/2011 7
F 3184
Are you a member?
This question is for testing whether or not you are a human visitor and to prevent automated spam submissions.
15 + 1 =
Solve this simple math problem and enter the result. E.g. for 1+3, enter 4.