Trosifol And Sentry Glass Join Forces

Clients and visitors to the Kuraray stand at Glasstec were met with a pleasant and inviting area to discuss in, and where they were presented with the recent developments following the takeover of DuPont's Glass Laminating Solutions(GLS)division. In this article, Glass-Technology was invited to a press meeting with the new Marketing Manager, Christoph Troska, who spoke about how work is now focused on maintaining close relationships with local markets, while also being more specific too.

Author
Un-named
Origin
Unknown
Journal Title
Glass-Tech Int 6/2014 42-47