Transparency Of Uv-Irradiated Uviol Glass

A study has been made of the effect of iron impurity on the transparency in the ultraviolet part of the spectrum of glass used for bactericidal lamps.

Author
V D Zolotkov Et Al
Origin
Svetotekhnika Glass Planning Org, A N Lodygin All-Union Inst Of Glass
Journal Title
Glass And Ceramics 1987 44 7-8 299-301
Sector
Special Glass
Class
S 115