Transition Metal Ions In Silicate Melts. Part 3. Nickel In Quenched Oxide Glasses

Optical absorption spectra characteristic of Ni2+ in octahedral coordination have been measured on glasses quenched from nickel bearing sodium silicate melts.

Author
C Nelson & W B White
Origin
Pennsylvania State University, Usa
Journal Title
Physics And Chemistry Of Glasses 34 5 1993 219-225