The Transfer Of Glass - Part 4: Transfer Of Glass Fragments From The Surface Of An Item To The Person Carrying It

The transfer of glass from the outer surface of a cardboard box to the clothing of a person carrying the box was investigated. In these experiments, the box was placed 1m behind a window which was subsequently broken. Glass was found on the box after all breakings, with more than 200 fragments on the surface in 7 out of 12 experiments. Between 1 and 22 fragments were recovered from the clothing (upper bodywear and legwear) of the person carrying the box. The distribution of fragment size and shape was similar to those described in previous studies.

Author
T J Allen Et Al
Origin
Forensic Science Service Dept, Birmingham, Uk
Journal Title
Forensic Science International 93 1998 201-208
Sector
Special Glass
Class
S 3665

Request article (free for British Glass members)

The Transfer Of Glass - Part 4: Transfer Of Glass Fragments From The Surface Of An Item To The Person Carrying It
Forensic Science International 93 1998 201-208
S 3665
Are you a member?
This question is for testing whether or not you are a human visitor and to prevent automated spam submissions.
4 + 9 =
Solve this simple math problem and enter the result. E.g. for 1+3, enter 4.